Zirconium Sponge

Zirconium Sponge

Packing:

  • 125 kg / Steel Barrel, Galvanized.

  • Sealed with Argon (Ar) gas.

Delivery:

  • 1 month

Zirconium Sponge in Steel Drum (4 x drums)

Chemistry Compositions, typical (wt. %, max):

Grade (Size: mm) Zr+Hf Hf Fe Cr Cl Al C N H O Others, total
XZr-1 (3~25) >99.4 2.3 0.032 0.0067 0.073 0.017 0.0061 0.0057 0.0037 0.083 0.10
XZr-3 (0~3) >95.0 3.0 0.193 0.023 0.167 0.058 0.048 0.148 0.0042 0.16 0.10

Size Distributions & Properties, typical:

Sponge Size || Sieving Analysis 0~1 mm 1~2 mm 2~3 mm 3~10 mm 10~25 mm Brinell Hardness (HB)
0~3 mm 25~35 % 50~30 % 25~35 % - - 129
3~25 mm - - - 40~60 % 60~40 % 126